Creasing Rules

Creasing Rules

Execution
Standard hardened and tempered creasing rule
HW hardness is achieved through modern cold-rolling technology

General
Only creasing rules with an exact profile geometry and tight height tolerances achieve
an excellent creasing result. Higher speeds are possible at automatic die presses and
folder-gluers, also for challenging materials.

Standard Creasing Rules
Execution HW Standard
Hardness min. 270 HV ~ 370 HV (≤ 3 pt)
Profile R, RD
Thickness 1.5 pt / 0.53 mm – 6 pt / 2.13 mm
Height 20.30 – 24.40 mm / 0.800˝ – 0.960˝

 

Tapered Creasing Rules
Execution Standard
Hardness ~ 370 HV
Profile RR
Thickness 2 / 1 pt · 2 /1.5 pt
Height 20.30 – 24.40 mm / 0.800˝ – 0.960˝

 

Heavy Top Creasing Rules
Execution Standard
Hardness ~ 370 HV
Profile RT, FRT, PT
Thickness 2/3 pt · 2/4 pt · 3/4 pt · 3/6 pt · 3/8 pt · 4/6 pt · 4/8 pt
Height 20.30 – 24.40 mm / 0.800˝ – 0.960˝

 